Self-levelling epoxy: thickness, coverage and where it fits

How self-levelling epoxy differs from a rolled coating and a cement levelling compound, how thick it goes on, how much you need per m², how long it takes to cure, and the floors it suits and the ones it does not.

The short answer

Self-levelling epoxy is a two-part resin poured onto a primed slab and spread to an even 2 to 3mm, where it flows out to a smooth, glossy finish with no joints. A rolled epoxy coating is far thinner, from about 0.14mm for a DIY kit to 1mm for a trade high-build coat. A cement-based self-levelling compound is a different product altogether: it flattens a floor before tiles or vinyl go down and is not made to be walked on as the finished surface. Self-levelling epoxy suits indoor kitchens, showrooms, garages and metallic floors on a flat, dry slab. It does not level a bumpy one.

"Self-levelling" is printed on three quite different products, and buying the wrong one is an expensive mistake. One is a resin floor finish, one is a thin rolled coating that is often sold alongside it, and one is a bag of cement powder for flattening floors before tiles go down. Here is what each one is, how thick it goes on, how much you need per square metre, how long it takes to cure, and where self-levelling epoxy is the right floor and where it is the wrong one.

Three products called self-levelling (scan this first)

Self-levelling epoxyRolled epoxy coatingCement self-levelling compound
What it isTwo-part resin, poured and spread, then spike rolledTwo-part epoxy paint, rolled on in one or two coatsCement powder mixed with water or latex, poured to flatten a floor
Typical thickness2 to 3mm (UK sheets run 1.5 to 4mm)About 0.14mm wet per coat on a DIY kit; trade coatings 0.15 to 1mm0.5 to 6mm on a common DIY bag
Is it the finished floor?YesYes, a thin oneNo: it goes under tiles, vinyl, lino, wood or carpet
Walk on itAbout 16 to 24 hours at 20°CAbout 16 hours at 20°CAbout 2 to 4 hours
Fully curedAbout 7 days at 20°C, about 10 at 10°CAbout 7 daysFloor covering can go on after about 8 hours
Will it fix an uneven slab?No, it mirrors what is under itNoYes, that is its job
Damp slabNo: under 75% RH, with a membraneNo: test firstWill not resist rising damp
OutdoorsNo, internal use onlyEpoxy yellows in sunlightThe common DIY bags are internal use only

Figures are from UK manufacturers' data sheets and the UK resin flooring trade body, FeRFA. Times are at 20°C unless stated, and every one of them gets longer in a cold room. The rest of this page explains each row.

What self-levelling epoxy actually is

Self-levelling epoxy, also called self-smoothing or flow-applied epoxy, is a two-part resin and hardener, usually 100% solids, often mixed with a fine filler. It is poured onto a primed floor, spread to a set thickness with a trowel or pin rake, then rolled with a spiked roller in two directions to let the air out. Because it is runny when mixed, the trowel marks flow out and it cures to a smooth gloss with no joints.

FeRFA sorts resin floors into eight types, and this is its Type 5, "flow applied flooring", which it notes is often called self-smoothing or self-levelling. Its typical thickness is 2 to 3mm. UK products sit around that: one Welsh-made system goes on at 2 to 3mm, a Sika product can be laid anywhere from 1.5 to 4mm, and a self-levelling epoxy sold to DIYers is usually laid at 1 to 2mm, up to 5mm in a single application.

The same pour is the base for most decorative floors. A plain solid colour resin floor is self-levelling epoxy in one colour with a topcoat, and a metallic epoxy floor is a self-levelling pour with metallic pigment worked through it while it is still wet. You can read how that effect is made in our piece on metallic epoxy flooring.

Self-levelling epoxy vs a rolled epoxy coating

A rolled coating is the same family of resin put on like paint. A typical DIY water-based epoxy kit covers about 7m² per litre in one coat, which works out at roughly 0.14mm of wet film. FeRFA puts trade floor coatings at 150 to 300 microns (0.15 to 0.3mm) and high-build coatings at 300 microns to 1mm, all in two or more coats. Even the thickest of those is a third to a half of a 2 to 3mm self-levelling pour, and most are a tenth or less.

Thickness is what you are paying for. A 2 to 3mm pour gives you a real body of resin, a flat-looking gloss and room for a metallic effect, where a coating is a fraction of a millimetre. If a coating is all your floor needs, our page on a concrete floor sealer against epoxy covers the cheaper end, and resin floor against floor paint covers why tins of floor paint lift.

Self-levelling epoxy vs a cement self-levelling compound

This is the easy one to get wrong. A cement-based self-levelling compound (the grey bags in every DIY shed) is for flattening an uneven floor before you lay something on it. One common UK bag is laid at 0.5 to 6mm, takes foot traffic in 2 to 4 hours, can be covered after 8, and says on its data sheet that it is not suitable as a final wearing surface. Its listed uses are under ceramic tiles, thermoplastic tiles, lino, wood block and carpet.

So the two do different jobs, and on a rough floor they can work together: level first, then pour the resin. The catch is that the resin maker has to accept what is underneath. Sika and Watco both tell you to level rough surfaces with their own levelling mortar or resurfacer before the self-levelling epoxy goes down, not with any bag that happens to be in stock.

How thick should resin flooring be?

It depends on what the floor has to take. For a home kitchen, showroom or garage, a 2 to 3mm self-levelling pour is the usual answer. A rolled coating of 0.15 to 1mm suits light use on a sound slab. Heavy industrial floors use the thicker types, from 4mm up. FeRFA's eight types give the whole ladder:

FeRFA typeWhat it isTypical thickness
1. Floor sealTwo or more thin coats, solvent or water borne150 microns
2. Floor coatingTwo or more coats, generally solvent free150 to 300 microns
3. High build coatingTwo or more coats, generally solvent free300 microns to 1mm
4. Multi-layerCoats with aggregate broadcast between themOver 2mm
5. Flow applied (self-levelling)Poured, smooth surface2 to 3mm
6. Resin screedTrowelled, heavily filled, sealed on topOver 4mm
7. Heavy duty flowablePoured, smooth surface4 to 6mm
8. Heavy duty resinTrowelled, filled all the way throughOver 6mm

A thousand microns is one millimetre, which is the conversion people trip on when comparing data sheets. For epoxy flooring specifically, the same ladder applies: a garage or kitchen at 2 to 3mm, an industrial floor thicker. Our step-by-step on how a resin floor is installed shows where each layer goes.

How much self-levelling epoxy you need per m²

Work it out by weight. One UK self-smoothing epoxy has a mixed density of 1.8kg per litre, and its sheet gives 3.6kg per m² at 2mm and 5.4kg per m² at 3mm. That is 1.8kg for every millimetre on every square metre, a sum you can run on any room:

  • Area in m² × thickness in mm × 1.8 = kilograms of mixed material.
  • A single garage of 18m² at 2mm: 18 × 2 × 1.8 = about 65kg.
  • The same garage at 3mm: about 97kg.
  • A 30m² kitchen and dining space at 2mm: about 108kg.

Those are theoretical figures, and both Sika and Virtus say so on their sheets: a porous slab, a rough profile, dips in the floor and spillage all eat more. The primer is extra too, and one system asks for two coats of it. Other products differ in density, so check the sheet for yours. A DIY kit listed at 5 to 10m² per 20kg at 1.5mm shows how wide the spread can be.

Worked out the kilos and lost your nerve?

A self-levelling pour gives you about 25 minutes per mix and no second go. Tell us the room size and the state of the slab, and we will price the full job in writing.

Where self-levelling epoxy suits

It is at its best on an indoor floor that is already flat, dry and sound, where you want a joint-free, wipe-clean gloss that takes daily wear. UK makers list food and drink production, retail and car showrooms, schools, hospitals, hotels, workshops and garages. In homes, that means:

  • Kitchens, where there are no grout lines to trap dirt. If the kitchen has underfloor heating, say so up front: Sika notes that underfloor heating or high temperatures combined with heavy point loads can leave dents in the resin, so the build is planned around it.
  • Showrooms and shops, where a high-gloss finish shows the stock off and cleans quickly.
  • Metallic floors, which need the poured body of a self-levelling floor for the effect to have any depth.
  • Commercial units and garages, where a floor with no joints is easy to sweep.

Light colours are worth a second thought where the sun hits. UK sheets warn that epoxy is not fully colour fast and can yellow under UV, most visibly in pale and blue shades. It does not weaken the floor, but it shows. Our page on whether an epoxy floor goes yellow covers the fixes.

Where it is the wrong choice

An out-of-level slab

Self-levelling epoxy levels itself, not your floor. A 2 to 3mm pour cannot fill a dip deeper than that, and a runny resin on a slab with a fall will drift towards the low side, thin out on the high side, and cure with the slope still in it. One UK maker puts it plainly on its sheet: flow-applied floors tend to mirror the imperfections in the slab underneath. It asks for the slab to meet SR1, which in FeRFA's flatness classes means no more than 3mm of gap under a 2m straightedge. If it does not, a scratch coat or levelling mortar goes down first.

To check your own floor, lay a 2m straightedge or a long spirit level in several directions and slide a 3mm drill bit under it. If the bit goes under in places, the slab needs levelling before resin. Cracks need sorting too; our page on putting resin over cracked concrete explains which ones matter, and what resin can be laid over covers tiles, screed and timber.

A damp slab

Moisture coming up through the concrete pushes resin off. FeRFA puts the limit for epoxy at 75% relative humidity, measured with a hygrometer, and UK sheets want an effective damp-proof membrane under the slab as well. Sika's own sheet says not to apply on substrates with rising moisture, and offers an epoxy-cement temporary moisture barrier where the slab tests too wet.

A quick DIY check, from a UK epoxy maker's own instructions: tape a sheet of plastic flat to the floor and leave it 24 hours. Droplets under the sheet, or darker concrete, mean moisture is coming through. That does not give you a number, but it tells you to stop and test properly. If a resin floor has already lifted, our page on epoxy floor problems goes through why.

Outdoors

UK flow-applied epoxy sheets mark it for internal use, and the makers warn that epoxy yellows in sunlight and must be kept dry while it cures. Outside, the answer is a UV-stable system or a different surface altogether: see outdoor resin flooring and, for parking, resin bound driveways.

How long self-levelling epoxy takes to cure

At 20°C, plan on about a day before you walk on it, two to four days before light traffic, and about a week to full cure. Cold slows every stage. One UK product's own table:

Floor temperatureFoot trafficLight trafficFull cure
10°CAbout 72 hoursAbout 6 daysAbout 10 days
20°CAbout 24 hoursAbout 4 daysAbout 7 days
30°CAbout 18 hoursAbout 2 daysAbout 5 days

A DIY self-levelling epoxy rates light traffic at 16 hours and parked cars at 48 hours at 20°C, with full chemical resistance at 7 days. The products above all need at least 10°C, and cold resin flows less, so the self-levelling part works less well too. Keep water off it for the first week, and keep the floor at least 3°C above the dew point or it can bloom with a cloudy film. If the room needs heating, Sika says to use electric warm-air heaters only: gas, oil and paraffin heaters give off water vapour and carbon dioxide that spoil the finish. If a floor stays tacky, see epoxy not curing.

Pot life shrinks as it warms: about an hour at 10°C, 30 minutes at 20°C and 15 minutes at 30°C on the same Sika product. That is the window to mix, pour, spread and spike roll each batch.

Can you lay self-levelling epoxy yourself?

Yes, DIY kits exist and some are sold for exactly this. What decides the result is everything before the pour. The slab has to be ground or shot blasted to take off the laitance (the weak, dusty top skin of the concrete), the cracks filled, the dust vacuumed up, the moisture tested and the primer put on. Then each batch has to be mixed, poured, spread to thickness and spike rolled inside its working time, with the next batch arriving before the edge of the last one starts to set. In a cold room the resin flows less, so trowel marks may not flow out before it sets.

Our walk-through on how to epoxy a garage floor covers the DIY steps, and is epoxy toxic covers the gloves, mask and ventilation the resin needs.

What we do before any resin goes down

Before a pour, the slab is diamond ground, every crack is filled and the dust is cleared. On a self-levelling floor the prep shows through more than on any other finish, because the gloss picks out every ridge it was poured over.

What a self-levelling epoxy floor costs

Published UK market rates put self-levelling epoxy at £40-£80 per m² supplied and laid, across four UK guides. A basic rolled coating runs £30-£60 per m², and a metallic finish £70-£150 per m². Grinding or shot blasting on a domestic job is often priced at £8-£20 per m² on top. Those are market ranges, not our prices. The full breakdown is in how much resin flooring costs.

Flat, dry and indoors? Then it is a pour

If your slab passes the straightedge and plastic-sheet checks, a self-levelling floor is a straightforward job. Send us the size and the room, and the price comes back in writing.

About this page

Who wrote this

The Obsidian Resin team wrote this. We prep and pour resin floors for kitchens, garages, showrooms and commercial units anywhere in Great Britain, self-levelling epoxy among them.

Why we wrote it

People ask for "self-levelling" and mean three different things, and the thickness and coverage figures they need are scattered across data sheets. This puts them in one place, from UK manufacturers' sheets and FeRFA's published floor types.

Our honest position

We would like to lay your floor, and that is our commercial interest in plain view. We have given the DIY answer straight, including the checks that tell you a self-levelling floor is the wrong one for your slab.

Frequently asked questions

How thick should resin flooring be?
For a home kitchen, garage or showroom, 2 to 3mm of self-levelling epoxy is the usual build, which is FeRFA Type 5. Rolled coatings are 0.15 to 1mm and suit lighter use. Heavy industrial floors go to 4 to 6mm or more.
How thick should epoxy flooring be?
A rolled epoxy coating is about 0.15 to 0.3mm, a high-build coating up to 1mm, and a self-levelling epoxy floor 2 to 3mm. UK self-levelling products range from 1.5 to 4mm, and heavy-duty flowable epoxy goes to 4 to 6mm.
Is self-levelling epoxy the same as self-levelling compound?
No. Self-levelling compound is cement-based and flattens a floor before tiles, vinyl, wood or carpet go down. A common UK one is laid at 0.5 to 6mm and is not made to be the finished surface. Self-levelling epoxy is resin and is the finished floor.
Will self-levelling epoxy level an uneven floor?
No. It levels itself, not the slab. At 2 to 3mm it cannot fill deeper dips, it drifts towards low spots, and it mirrors what is under it. UK makers want the slab within 3mm under a 2m straightedge, or levelled first with their own levelling mortar.
How much self-levelling epoxy do I need per m²?
About 1.8kg per m² for every millimetre on a typical UK product, so 3.6kg per m² at 2mm and 5.4kg at 3mm. An 18m² garage at 2mm needs about 65kg before wastage and primer. Check the density on the sheet for your product.
How long does self-levelling epoxy take to dry?
At 20°C, about 16 to 24 hours to walk on, two to four days for light traffic and about seven days to full cure. At 10°C one UK product takes about 72 hours to walk on and 10 days to full cure.
Can you use self-levelling epoxy outside?
No. UK flow-applied epoxies are made for internal use, and epoxy yellows in sunlight. Outdoors needs a UV-stable system or a different surface, such as resin bound for a drive.
Can you put self-levelling epoxy on a damp floor?
No. Epoxy needs the slab under 75% relative humidity and a damp-proof membrane beneath it. Where a slab tests too wet, some makers offer a moisture barrier system to go down first.
How thick should a resin bound driveway be?
That is a different product: resin mixed with stone and laid over a base. One UK manufacturer gives a typical depth of 16 to 20mm over concrete or asphalt, depending on the stone size. Our resin bound driveways page has the detail.

Read enough? Send us the space and your postcode, and get the written figure for your own floor or driveway.